Preparation, Characterisation, and Photocatalytic
Behaviour of - with Visible Light Response
Figure 6
Time required for the photodegradation of 1 mM 4-chlorophenol
in aqueous suspensions of Co(x%)-TiO2 as a function of the amount of cobalt (x%). The final calcination temperature
was 400°C for 30 minutes.