Optical Absorption Enhancement in Amorphous Silicon Films and Solar Cell Precursors Using the Aluminum-Induced Glass Texturing Method

Figure 1

AFM image of the AIT sample after TCO deposition. (a) is the 2D top view and (b) is the 3D projection of the AFM measurement. The -axis scale is not proportional to the scales of the - and -axis.