Research Article
Creep Rupture Behavior in Dissimilar Weldment between FB2 and 30Cr1Mo1V Heat-Resistant Steel
Figure 3
SEM fractograph which shows secondary cracks, inclusions, and local ductile fraction in the specimen after creep test at 783 K (510°C) under 320 MPa.