Research Article
Preparation of Luminescent Glass Aggregates from Soda-Lime Waste Glass
Figure 1
XRD patterns of bare phosphor and phosphor-in-glass ceramic aggregates with varying phosphor contents. The samples were sintered at 750°C for 30 min. The image in (b) is a zoom for CaSiO3 and SiO2 XRD peaks.