Mechanism and Optimized Process Conditions of Forming One-Dimensional ZnO Nanorods with Al-Doping by Electrodeposition Method

Figure 2

X-ray diffraction patterns of the ZnO samples formed on FTO substrates by electrodeposition method at a constant potential -1.5 V from 3 mM Zn(NO3)2 aqueous solutions containing Al(NO3)3 with different Al3+/Zn2+ ratio in the bath: (a) 0 at%, (b) 1 at%, (c) 2 at%, and (d) 3 at%, at 80°C for 60 min with a fixed electrode distance of 2 cm.