Figure 6

The tensile stress-strain curves of PLA/PBAT blends recorded at room temperature (27°C). (a) Untreated, (b) Annealed at 100°C for 8 hrs, (c) annealed at 100°C for 24 hrs.
951696.fig.006a
(a)
951696.fig.006b
(b)
951696.fig.006c
(c)