Research Article

Influence of Thickness on the Holographic Parameters of H-PDLC Materials

Figure 4

(a) Diffraction efficiency as a function of recording exposure; sample thickness between 14 and 20 m using composition 1. (b) Diffraction efficiency as a function of recording exposure; sample thickness between 23 and 37 m using composition 2.
(a)
(b)