Research Article
Use of Rubber Process Analyzer for Characterizing the Molecular Weight Parameters of Natural Rubber
Figure 3
Stress relaxation curves of natural rubber at 100°C (⋄: milled 5 times; □: milled 10 times; △: milled 15 times; ×: milled 20 times; +: milled 25 times; ○: milled 30 times).