Research Article
Influence of the Initial Fiber Orientation on the Weld Strength in Welding of Glass Fiber Reinforced Thermoplastics
Table 4
Selected design points in hot plate welding.
| | Design point | | | [mm/s] | [°C] |
| | I | 0.34 | 0.75 | 5 | + 80 K | | II | 0.2 | 0.6 | 1 | + 60 K | | III | 0.34 | 0.75 | 9 | + 80 K | | IV | 0.48 | 0.75 | 5 | + 80 K | | V | 0.48 | 0.9 | 9 | + 100 K | | VI | 0.34 | 0.75 | 5 | + 100 K |
|
|