Research Article
Influence of Fiber Content on Mechanical and Morphological Properties of Woven Kenaf Reinforced PVB Film Produced Using a Hot Press Technique
Figure 12
The SEM micrographs of the Charpy impact failure surfaces of kenaf/PVB film composite.
| (a) 10% kenaf weight |
| (b) 20% kenaf weight |
| (c) 30% kenaf weight |
| (d) 40% kenaf weight |
| (e) 50% kenaf weight |
| (f) 60% kenaf weight |