Research Article
Cracking Behaviour of Alkali-Activated Aluminosilicate Beams Reinforced with Glass and Basalt Fibre-Reinforced Polymer Bars under Cyclic Load
Table 8
Bending moment at cracking, ultimate and service state.
| Specimen ID | Experimental moments (kNm) | Cracking moment (Mcr) | Ultimate moment (Mu) | Service moment | 2000 με | (0.3 Mu) |
| BRGC-C | 1.50 | 8.70 | 2.25 | 2.61 | GRGC-C | 1.50 | 6.83 | 1.5 | 2.05 | SRCC-C | 3.75 | 11.14 | 3.75 | 3.34 | BRGC-S | 2.25 | 8.36 | 3.75 | 2.51 | GRGC-S | 1.50 | 8.10 | 2.25 | 2.43 | SRCC-S | 3.75 | 12.45 | 5.00 | 3.74 |
|
|