Research Article

Fabrication and Properties of Polycaprolactone/Poly(Butylene Succinate) Blends Based on Electrospinning

Table 1

Concentration of electrospinning solution.

Serial NumberSpinning fluid composition (mass ratio)The mass fraction (%)Spinning voltage (kV)Push the note rate (mL/h)

1PCL/PBS = 1 : 16120.8
2PCL/PBS = 1 : 18120.8
3PCL/PBS = 1 : 110120.8
4PCL/PBS = 1 : 112120.8