[Retracted] Nondestructive Testing of Coal Mine Wire Ropes Based on Magnetic Sensors
Table 3
The relationship between fatigue damage and magnetic parameters.
| Cycles | Saturation magnetic induction | Remanence | Residual strength |
| 1 | 2176.4 | 771.3 | 70.2 | 3 | 2173.2 | 766.8 | 67.3 | 5 | 2171.8 | 763.5 | 65.5 | 7 | 2170.1 | 761.4 | 63.1 | 9 | 2168.3 | 760.2 | 62.2 | 11 | 2164.9 | 759.3 | 61.4 | 13 | 2162.1 | 757.6 | 60.6 | 15 | 2160.7 | 755.8 | 59.3 | 17 | 2158.5 | 753.7 | 58.0 |
|
|