Research on the Characteristics and Mechanism of the Cumulative Release of Antimony from an Antimony Smelting Slag Stacking Area under Rainfall Leaching

Table 2

Cumulative release amount of Sb in smelting slag under different rainfall duration.

Duration (h) Sb release content (mg/kg)
123456789101112

4.06.337.368.157.8610.099.187.138.259.3210.238.257.2399.35
6.08.6210.4913.0713.8116.3015.1113.5712.3614.59000117.92
8.011.808.747.507.2212.5210.0013.580000071.36
12.019.6420.5623.9623.5625.630000000113.35