Research Article
Study on Blending of Wall Material of the Nonel Tube by CSW/PE-g-MAH
Table 4
Thermal degradation parameters for LDPE/CSW/PE-g-MAH composites.
| | Sample | To (°C) | Tp (°C) | αp (%) | (dα/dT)p (% (°C)) | W600 (%) | Char (%) |
| | 100/0/0 | 428.92 | 470.34 | 58.66 | 2.616 | 0.17 | 0.03 | | 85/15/0 | 428.25 | 473.33 | 54.35 | 2.253 | 16.69 | 16.57 | | 84/15/1 | 437.08 | 472.98 | 47.73 | 2.453 | 16.27 | 16.21 | | 80/15/5 | 442.73 | 483.43 | 55.45 | 2.421 | 18.67 | 18.51 |
|
|