Photodegradation of TA in as-prepared samples, (b) the kinetic curves, and (c) the pHPZC determination of N-ZnO. The reaction conditions: dosage catalyst 0.5 g/L, tartrazine concentration of 20 mg/L, and pH = 6.0.
| (a) |
| (b) |
| (c) |