Research Article

Preliminary Examination of the System Fly Ash-Bottom Ash-Flue Gas Desulphurization Gypsum-Portland Cement-Water for Road Construction

Figure 1

XRD diffractograms of the mixture FA-PC-FGD gypsum-BA-W.
421480.fig.001a
(a)  FA consisted of coarser particles (<1.651 mm), after 7 days
421480.fig.001b
(b) FA consisted of coarser particles (<1.651 mm), after 28 days
421480.fig.001c
(c) FA consisted of smaller particles (<0.42 mm), after 7 days
421480.fig.001d