Research Article

Electrophoretic Deposition of Aluminum Nitride from Its Suspension in Acetylacetone Using Iodine as an Additive

Figure 5

(a) SEM micrograph of bare Al substrate. (b) SEM micrograph of an AlN coating on Al cathode for electrophoretic deposition of AlN in 0.2 g/L I2/acetylacetone at a potential of 20 V. Deposition time and the amount of AlN in the suspension are 5 min and 10 g/L, respectively.
489734.fig.005a
(a)
489734.fig.005b
(b)