Producing Polymer Fibers by Electrospinning in Supercritical Fluids
Figure 3
SEM of PVP fibers created by electrospinning a 5 wt% solution into N2 at 298 K and 0.1 MPa: (a) N2-ethanol solution; (b) N2-DCM solution; and (c) simulated binary phase equilibrium for N2-ethanol and N2-DCM solutions.