Table 2

Water uptake of EDC/NHS- and GDA-crosslinked HA coatings ( ) after different swelling times in 1 mL PBS/Tween 20. Data shown in mg water per mg coating as mean ± SD.

Swelling timeEDC/NHS-crosslinked
HA coating
GDA-crosslinked
HA coating

1 min5.04 ± 0.171.90 ± 0.25
2 min5.27 ± 0.702.61 ± 0.15
1 h6.78 ± 0.393.21 ± 0.33