Research Article

Characteristics of the Ti1.27Fe + 11 wt.% Ni Composite Obtained by Arc Melting and Ball Milling

Figure 3

SEM micrographs of Ti1.27Fe/Ni at different stages of processing: (a) Ti1.27Fe alloy-as melted, (b) homogenized, (c) TiFe + 11 wt.% Ni after 5 h of ball milling, and (d) hydrogenated composite.
831853.fig.003a
(a)
831853.fig.003b
(b)
831853.fig.003c
(c)
831853.fig.003d
(d)