Research Article

Characteristics of the Ti1.27Fe + 11 wt.% Ni Composite Obtained by Arc Melting and Ball Milling

Figure 4

TGA profile (—) and its derivative (- - -) of hydrogenated Ti1.27Fe + 11 wt.% Ni composite indicating wt.% H2 released as function of the temperature.
831853.fig.004