The Online Research of B2O3 on Crystal Behavior of High Ti-Bearing Blast Furnace Slag

Figure 6

Area scanning mapping of Ti, Ca, Si, Mg, Al, O, and EDS in 0# sample without B2O3 at 1485°C.