Research Article

Hybrid Deep Eutectic Solvent of LiTFSI-Ethylene Glycol Organic Electrolyte for Activated Carbon-Based Supercapacitors

Table 3

Oxidation and reduction limit potentials of mixture DES 1 : 4 + x% wt. AN and DES 1 : 4 + y% wt. EC.

x (%)Eanode (V)Ecathode (V)yEanode (V)Ecathode (V)

0% wt. AN4.522.550% wt. EC4.522.55
10% wt. AN4.552.4310% wt. EC4.662.42
20% wt. AN4.582.4220% wt. EC4.652.42
30% wt. AN4.582.6430% wt. EC4.672.41
50% wt. AN4.492.7350% wt. EC4.552.41

ibackground for Ecathode = 0.02 mA, ibackground for Eanode = 0.002 mA. : the potential value is versus Li+/Li.