Research Article
Recycling of Iron Slag Waste in the Production of Ceramic Roof Tiles
Table 3
Comparison between the properties of the suggested sample and standard values.
| ||||||||||||||||||||||||||||||||
Freeze-thawing tests were not carried out for samples fired at 1100°C, although they would have almost certainly passed the test because of their superior properties over those fired at 1000°C. |