Research Article

Synthesis of Spherical Composite CMC-LTO-EGDE-ME for Lithium Recovery from Geothermal Water

Table 1

Chemical composition of the geothermal water sample.

pHComposition (mg·L−1)
Li+Na+K+Rb+Cs+Ca2+ClB2O3

8.8025.78682.01137.93.4517.58211.05973.06360.16