Research Article

Synthesis of Spherical Composite CMC-LTO-EGDE-ME for Lithium Recovery from Geothermal Water

Table 2

Selectivity of the spheres CMC-LTO-EGDE-ME in geothermal water.

Li+Na+K+Ca2+Cs+

K d (mL/g)3766.7020.7034.3996.1774.83
α (Li/Me)1.00181.97109.5339.1750.34