Synthesis of Spherical Composite CMC-LTO-EGDE-ME for Lithium Recovery from Geothermal Water

Table 5

Parameters of intraparticular diffusion model.

K dif1 (mg/g·h1/2)r 1K dif2 (mg/g·h1/2)r 2K dif3 (mg/g·h1/2)r 3

4.5830.9962.5180.9981.0180.989