Synthesis of Spherical Composite CMC-LTO-EGDE-ME for Lithium Recovery from Geothermal Water
Table 6
Comparison of the Li+ adsorption capacity and equilibration time at the different initial contents and water samples.
| Adsorbent | Sample | Li+ content (mg·L−1) | Adsorption capacity (mg·g−1) | Equil. time (h) | Refs. |
| HMO/Al2O3 | Seawater | 30 | 15 | 499 | [30] | Chitosan/HMO | Seawater | 30 | 11.4 | 168 | [31] | H1.6Mn1.6O4/PAN | LiCl/LiOH solution | 35 | 10.3 | 24 | [32] | LiMnO2/PVA | LiOH solution | 7 | 6.9 | 24 | [33] | CTS/HMO | Geothermal water | 25.78 | 8.98 | 24 | [3] | HTO-400 | Li+ solution | 200 | 34.2 | 24 | [34] | HTO-Am | LiCl solution | 300 | 50.03 | 24 | [35] | H4Ti5O12 | Li+ solution | 500 | 52.97 | 1 | [36] | CMC-HTO-EGDE | Geothermal water | 25.78 | 12.01 | 8 | This work |
|
|