Effect of paint liquid solid content on paint film appearance and film thickness (25°C).
| Paint liquid solids (%) | 50 | 45 | 40 | 38 | 35 | 33 | 30 |
| Reference viscosity (s) | 70–100 | 60–90 | 45–70 | 33–40 | 30–36 | 28–33 | 22–30 | Cold rolled sheet film thickness (μm) | 35–40 | 30–36 | 24–30 | 20–24 | 18–22 | 15–20 | 13–15 | Appearance of cold-rolled sheet | Difference | Difference | Better | Better | Good | Good | Good | Hot rolled sheet film thickness (μm) | 45–60 | 40–55 | 30–45 | 25–35 | 22–30 | 20–26 | 18–22 | Appearance of hot rolled sheet | Difference | Difference | Better | Better | Good | Good | Good | Hot rolled sheet film thickness (μm) | 50–70 | 45–60 | 40–55 | 35–45 | 30–40 | 25–35 | 20–30 | Appearance of hot rolled sheet | Difference | Difference | Better | Better | Good | Good | Good |
|
|