Control of dipping bath liquid, parameter changes, and their influence on the paint film.
| Process parameters | Detection frequency | Question | Ills | Countermeasures |
| Solid content, 33%–40% | 1 Time/day | High | Film thickness, flow marks, pinhole bubbles | Add original paint | Low | Film Thickness, Shrinkage, Bottom Exposed | Add pure water |
| Viscosity, 28–45 s | 2 Times/class | High | Flow marks, fat edges | Add pure water, solvent | Low | Shrinking, film thin | Add original paint |
| pH, 8–10 | 2 Times/week | High | | | Low | Pigment settles and the system deteriorates | Refill original paint, amines |
| Temperature, 15–30°C | 2 Times/class | High | Paint film sagging | Chilled water cooling | Low | Flow marks, fat edges, matte paint film | Heat exchange cooling |
|
|