Research Article
Experimental Study on Chloride Stress Corrosion Cracking Sensitivity of 316L Stainless Steel
Figure 10
SEM images of fracture surface morphology of tensile test coupons (Pco2 = 0.1 Mpa, T = 65°C): (a) Cl− = 60,000 mg/L; (b) Cl− = 80,000 mg/L.