Research Article

Preparation and Characterization of Biodegradable Composited Films Based on Potato Starch/Glycerol/Gelatin

Table 4

The factor loading matrix of three components.

IndexPrincipal componentsPercentage (%)
123

T%0.514−0.5380.57513
Thickness(mm)0.8440.4750.06234
E%0.7720.313−0.52018
TS (MPa)0.0380.7050.66230
WS (%)0.668−0.5860.0415

− indicated negative correlative.