Research Article

Time-Resolved 2PPE and Time-Resolved PEEM as a Probe of LSP's in Silver Nanoparticles

Figure 9

TR-2PPE measurement of the 2D nanoparticle array with perpendicular light incidence showing the 2PPE count rate and the FWHM of the corresponding cross-correlation trace with respect to the polarization angle (in respect to the direction of the long axis).
249514.fig.009