Nanoporous Calcium Silicate and PLGA Biocomposite for Bone Repair
Figure 10
H&E stained section of n-CPC scaffolds implantation into bone defects of rabbit femora for 2 (a), 4 (b), 8 (c), and 12 weeks (d). M represents gradually degraded materials, and B represents new bone tissue, respectively.