Research Article

Stable Aqueous Suspension and Self-Assembly of Graphite Nanoplatelets Coated with Various Polyelectrolytes

Table 2

Atomic concentration of the surface of xGnP before and after PE modification.

C1sO1sS2pN1sZr3d

xGnP92.386.380.25
SPS-xGnP94.314.510.760.22
SPS-xGnP redispersed*91.716.440.790.20
PEI-xGnP91.844.733.190.25
PEI-xGnP redispersed*90.695.793.240.28

*The xGnP was redispersed in DI water with mild sonication for 10–15 minutes, and then filtrated and dried before XPS measurement.