Research Article

Nanocrystalline Pb(Zr0.52Ti0.48)O3 Ferroelectric Ceramics: Mechanical and Electrical Properties

Figure 3

Transmission electron micrographs of PZT samples with 30 hours and 40 hours of milling time.
783043.fig.003a
(a)
783043.fig.003b
(b)