TEM images of the detached nanoparticles from the GP product with the SEAD pattern images. The TEM image of the Ni nanoparticles was observed at a size of 50 nm in (a). The insert (b) shows the EDS results, which confirmed the presence of nickel in the nanoparticle. (c) HR-TEM image of the nanoparticle. The insert (d) shows the SAED pattern along the (111) zone axis, which confirmed the single crystal structure of nickel. Representative images were shown after the experiments were performed in triplicate.