Tunable Structures and Properties of Electrospun Regenerated Silk Fibroin Mats Annealed in Water Vapor at Different Times and Temperatures
Figure 6
Breaking strength and breaking energy of electrospun RSF mats treated with water vapor: (a) at 65°C for different times; (b) for 3 h at different temperatures.