Research Article
Study of Tribological Properties of Nanolamellar WS2 and MoS2 as Additives to Lubricants
Table 1
Profilometer results of wear scar.
| Sample | Wear scar depth (μm) | Wear volume (μm3·10−3) |
| WS2-NL | 0.48 | 3.1 | MoS2-NL | 0.42 | 2.0 | MoS2-C | 0.57 | 3.5 | WS2-NL (400°C) | 2.87 | NA | MoS2-NL (400°C) | 3.49 | NA | Oil | 0.82 | 74.8 | Oil + 5 wt.% WS2-NL | 0.57 | 30.3 | Oil + 5 wt.% MoS2-NL | 0.56 | 15.1 | Oil + 5 wt.% MoS2-C | 0.75 | 46.7 |
|
|