Research Article

Halo Evolution of Hypereutectic Al-17.5Si Alloy Treated with High-Current Pulsed Electron Beam

Figure 2

SEM micrographs of halo of HCPEB-treated Al-17.5Si alloy under different pulse numbers.
(a) 5 pulses at low magnification
(b) 5 pulses at high magnification
(c) 15 pulses at high magnification
(d) 25 pulses at high magnification