Responsivity Dependent Anodization Current Density of Nanoporous Silicon Based MSM Photodetector

Figure 2

XRD patterns of NPSi samples grown at various anodization current densities: 20 mA/cm2, 25 mA/cm2, and 35 mA/cm2.