Research Article

The Pore Confinement Effect of FDU-12 Mesochannels on MoS2 Active Phases and Their Hydrodesulfurization Performance

Table 1

Textural and structural characteristics of FDU-12 support, Mo()/FDU-12, Mo(10)/SBA-15, and Mo(10)/γ-Al2O3 catalysts.

Sample (m2/g) (cm3/g) (nm)

FDU-12346.40.9017.4 (8.7)
Mo(6)/FDU-12325.50.8717.2 (8.6)
Mo(8)/FDU-12316.80.8217.2 (8.6)
Mo(10)/FDU-12310.10.7917.2 (8.5)
Mo(12)/FDU-12296.30.7617.1 (8.5)
Mo(15)/FDU-12268.90.6816.8 (8.4)
Mo(10)/SBA-15623.50.817.1
Mo(10)/γ-Al2O3226.10.355.9

Note: specific surface area calculated by BET method, pore volume, pore diameters calculated from the adsorption branch, and window sizes obtained from the desorption branch by using the BJH method.