Pressure and permeability before and after α-ZrP-I injection.
| Number | Concentration (mg/l) | 1 (MPa) | 2 (MPa) | 1 (×10−3 μm2) | 2 (×10−3 μm2) | Pressure drop rate (%) | 2/1 |
| 1 | 20 | 0.3527 | 0.3348 | 3.08 | 3.25 | 0.05 | 1.05 | 2 | 50 | 0.3614 | 0.1907 | 3.01 | 5.70 | 47.23 | 1.89 | 3 | 100 | 0.3703 | 0.4006 | 2.93 | 2.71 | −8.18 | 0.92 | 4 | 200 | 0.2815 | 0.5024 | 3.86 | 2.16 | −78.47 | 0.56 |
|
|