Research Article

Effects of Sintering Temperature on the Morphology and Photoluminescence of Eu3+ Doped Zinc Molybdenum Oxide Hydrate

Figure 2

XRD curves of Eu3+ doped ZnMoO4 compounds obtained by thermal annealing the precursor at 400°C (a), 600°C (b), and 800°C (c) for 2 h.