Research Article
Effects of Sintering Temperature on the Morphology and Photoluminescence of Eu3+ Doped Zinc Molybdenum Oxide Hydrate
Figure 8
Absorption spectra of undoped ZnMoO4 (blue curves) and Eu3+ doped ZnMoO4 (red curves). The undoped ZnMoO4 and Eu3+ doped ZnMoO4 nanoplates were derived by sintering their precursors at 600°C for 2 h, respectively. Inset: Tauc plot of the undoped ZnMoO4 obtained by sintering its precursor at 600°C for 2 h.