Effects of Sintering Temperature on the Morphology and Photoluminescence of Eu3+ Doped Zinc Molybdenum Oxide Hydrate
Figure 9
Time-resolved PL spectra of ZnMoO4:Eu3+ derived by sintering the precursor at 600°C for 2 h. The emission wavelength was fixed at 550 nm (a) and 615 nm (b), respectively.