Research Article

Micromorphology and Mechanical and Dielectric Properties of Bismaleimide Composite Modified by Multiwalled Carbon Nanotubes and Polyethersulfone

Table 2

Impact strength and bending strength of the composite.

TypeImpact strength (kJ/m2)Increasing rate (%)Bending strength (MPa)Increasing rate (%)

A9.230100.320
B010.3612.24117.3616.99
B113.3744.85124.0923.69
B216.0974.32153.5753.08
B314.4156.12128.6428.22
B412.7337.92121.0420.65