High-Temperature Conductive Stability of ITO/Pt Bilayer-Film Electrode for Applications in High-Temperature SAW Devices
Figure 5
SEM images of the Pt film electrodes after annealing at 1000°C for (a) 5 min, (b) 10 min, (c) 15 min, (d) 20 min, (e) 25 min, (f) 30 min, (g) 35 min, (h) 40 min, and (i) 45 min.