Research Article
High-Temperature Conductive Stability of ITO/Pt Bilayer-Film Electrode for Applications in High-Temperature SAW Devices
Figure 6
SEM images of the ITO/Pt film electrodes after annealing at 1000°C for (a) 0.5 h, (b) 1 h, (c) 1.5 h, (d) 2 h, (e) 2.5 h, (f) 3 h, (g) 3.5 h, and (h) 4 h.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |
(h) |